High performance composite material

The high performance composite material is the HTC-series product and uses glass and carbon fiber. It is applied in various fields by forming high-strength special composite materials with filament winding, laminate, and pultrution methods, and has excellent mechanical strength, heat resistance, and workability.
  • High performance composite material
  • High performance composite material
  • High performance composite material
Product Name Mix Ratio Viscosity(cps,25℃) Tg(℃) Curing condition Application
HTC-1375
100:30
12,000~1,3000
100~200
120~130(Tg) 120℃x 6hr
Good weather & chemical resistance
Glass fiber & carbon fiber filament Winding,
Laminate for vessel & chemical plant
HTC-1370
100:25
12,000~1,3000
800~1,200
170~180(Tg) 120℃x2hr+
170℃x 6hr
Excellent weather & chemical resistance
Glass fiber & carbon fiber filament Winding,
Laminate for vessel & chemical plant
HTC-1350
100:100
7,000~10,000
50~70
150~160(Tg) 100℃x2hr+
140℃x 6hr
Excellent thermal & chemical resistance.
Excellent electrical properties.
Glass fiber & carbon fiber filament Winding
HTC-1330
100:90
12,000~13,000
50~70
130~140(Tg) 100℃x2hr+
120℃x 5hr
Excellent chemical resistance &
electrical properties.
Glass fiber & carbon fiber filament Winding
HTC-1320
100:80
12,000~13,000
50~70
120~130(Tg) 100℃x2hr+
120℃x 5hr
Excellent chemical resistance &
electrical properties.
Glass fiber & carbon fiber filament Winding
HTC-1310
100:70
10,000~12,00
50~70
80~90(Tg) 100℃x2hr+
120℃x 5hr
Excellent crack resistance
Glass fiber & carbon fiber filament Winding (>50T)
HTC-1039
100:20
7,500~8,500
10~30
125~135(Tg) 100℃x1hr
Low chlorine environment-friendly carbon fiber laminate.
Excellent weather resistance & electrical properties.
HTC-1039F
100;25
9,000~11,000
10~30
85~95
100℃x2hr
Flame retardancy carbon fiber laminate
Excellent electrical & mechanical properties.
HTC-1035 일액형 60~120 110~120(Tg) 130℃×4h Glass fiber & carbon fiber composite prepreg
HTC-670 100 : 90 : 2 1,000~2,000
50~150
110~120(Tg) (80℃×2h)+
(140℃×8h)
Transformer filament winding
HTC-650 100 : 10 Paste
400~500
70~80 25℃x (12~24)h High strength Gel Coat
HTC-665C 100 : 50 10,000~15,000
150~350
70~80 25℃×24 or
60℃×2h
Laminate & Filament Winding
HTC-667C 100 : 25 300~500
400~600
80~90 25℃×24h or
60℃×2h
LLaminate & Filament Winding
100 : 50 1,500~2,500
100~200
80~90 25℃×24h or
60℃×2h
Laminate & Filament Winding
HTC-2300 100 : 100 3,000~6,000
50~150
120~130 (Tg) 130℃×5h Pultrusion